Anodizing

chemicals for aluminum anodizing, powder coating and steel passivation

AD-A01 Rapid Anodization Additive

AD-A01 Rapid Anodization Additive

Anodizing

Wide temperature Rapid anodic oxidation additive can make oxidation process can be carried out in 18-30 ℃ interval, reduce cooling system refrigeration pressure, speed up film forming speed and save electric energy.

Address No. 26, Changgang South Road, Shishan Town, Nanhai District, Foshan City, Guangdong Province, China

Phone + 86-757-81093737

E-mail lizzie@andonchem.com export@andonchem.com

1.It can work under temperature range of 18-35 ℃ and no chilling required, can use tap water directly. 

2.Oxidation current between 1.0-3.0A/dm2

3.The AL3 +, Cu2 +, Fe3 + tolerance is more then double. Oxidation rate also increased to 0.4~1.0μm/min.


Free acid  :  140~160g/l   AL³+ :1~30g/l   AD-A01: 35±5 g/l        Current density :1.0~2.0A/dm2                     Voltage  :10~18 V Temperature :20~35℃

Acid :150~180g/l

AD-A01: 35±5 g/l

Swisstek-Logo
Sapa-Logo
Lanka-Logo
Ic-interCairo-Logo
Hydro-Logo
Dyson-Logo
CMR-Logo
Alumex-Logo